Waterproofing Engineering

Waterproofing Issues

Engineering assessment of waterproofing failures and water ingress for podium decks, basements, roofs and wet areas - with engineered remediation design.

Request Assessment WhatsApp Us

Typically replies within 2 hours

Engineer inspecting a building envelope for water ingress and waterproofing failure in the UAE

Quick Answer

New Nordic assesses waterproofing failures across podium decks, basements, roofs and wet areas - diagnosing why the system failed and engineering a remediation that lasts, rather than recoating over the same problem.

Because water drives structural deterioration, we assess both the waterproofing failure and the concrete damage it has caused, then design a durable fix.

Who This Is For

  • - Building owners & OAs
  • - Facility managers
  • - Developers in defects-liability
  • - Contractors

When It Is Needed

  • - Basement or deck leaks
  • - Failed roof membranes
  • - Recurring wet-area damp
  • - Before re-waterproofing

What Problems This Service Solves

Waterproofing failures are an engineering problem, not just a coating problem. Diagnosing why the system failed is what makes the repair last.

Podium & Deck Failures

Podium and deck membranes fail at details and movement joints. We locate the breaches and assess the substrate.

Basement Water Ingress

Below-grade water pressure defeats inadequate tanking. Assessment identifies the failure mechanism and remedy.

Roof Membrane Breakdown

UV, heat and movement degrade roof systems. We assess the system's condition and remaining life.

Consequential Concrete Damage

Long-term leakage corrodes reinforcement. We assess the structural damage behind the waterproofing failure.

Repeat Recoating Failure

Recoating without diagnosis fails again. Root-cause engineering ends the cycle.

Wrong System Selection

The wrong waterproofing system for the exposure guarantees failure. We specify the correct engineered solution.

The Assessment Process

01
1

Proposal

Scope and diagnostic plan within 48h

02
2

Failure Survey

Mapping of leakage and waterproofing defects

03
3

Diagnostic Testing

Moisture, flood and adhesion testing

04
4

Root-Cause Analysis

Why the system failed and what it damaged

05

Remediation Design

Engineered waterproofing specification

Methods & Equipment

Diagnostic testing and remediation design are delivered in-house, so the cause of failure and its cure stay with one accountable team.

Flood & Spray Testing

Controlled testing to locate breaches in the waterproofing.

Moisture Mapping

Quantifies dampness within decks, slabs and walls.

Infrared Thermography

Reveals water tracking and membrane defects non-intrusively.

Adhesion Testing

Assesses bond and condition of existing membranes.

Half-Cell Potential

Assesses corrosion in concrete damaged by leakage.

Core Sampling

Confirms substrate condition beneath the waterproofing.

What You Receive

Every New Nordic engagement produces bespoke engineering deliverables - not a template. Where applicable, work is stamped by a qualified professional engineer and accepted by Dubai Municipality.

Assessment Report

PE-stamped waterproofing failure diagnosis

Failure Mapping

Located breaches and failure mechanisms

Remediation Specification

Engineered waterproofing system design

Substrate Assessment

Condition of the concrete beneath the system

Test Evidence

Flood-test, moisture and thermographic data

Supervision Support

Site supervision of the remediation in-house

Why New Nordic

In-House NDT Equipment

All key equipment owned and operated in-house - no delays waiting for subcontractors.

48h Mobilization

Engineers on site within 48 hours of signing for urgent structural work.

PI Insurance Active

Professional Indemnity Insurance active on all engagements. Client protection built in.

One Responsible Partner

From inspection to certification to remediation - single accountability throughout.

Frequently Asked

Why does my waterproofing keep failing?

Usually because repairs recoat the surface without diagnosing why the system failed - at details, joints or the substrate. Root-cause assessment ends the cycle.

Do you assess the concrete underneath?

Yes. Long-term leakage corrodes reinforcement, so we assess both the waterproofing failure and any consequential structural damage.

Can you design the remediation?

Yes. We specify an engineered waterproofing system suited to the exposure and can supervise its installation.

Which areas do you cover?

Podium decks, basements and tanking, roofs, balconies, wet areas and any structure where waterproofing has failed.

How is this different from a leak investigation?

It focuses specifically on waterproofing system failure and its remediation, often alongside our building envelope leakage investigation.

Ready to Start

Talk to Us About Waterproofing Issues

Send us your building details. Our engineers will review and provide a detailed proposal within 48 hours.

Request Assessment WhatsApp

Typically replies within 2 hours

Ready to get started?

Book Your Priority Assessment

Avoid last-minute compliance pressure and rejected reports. New Nordic provides inspection, testing, reporting and certification through one accountable engineering team.

Typically replies within 2 hours

Call Now WhatsApp